http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108178957-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2227 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1662 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 |
filingDate | 2017-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-06-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108178957-B |
titleOfInvention | Baking-free glaze-imitating coating and preparation method and application thereof |
abstract | The invention discloses a baking-free glaze-imitating coating as well as a preparation method and application thereof, wherein the baking-free glaze-imitating coating comprises the following components in parts by weight: 28-35 parts of organic silicon modified acrylic resin, 26-32 parts of polyurethane modified organic silicon resin, 3-5 parts of silane coupling agent, 3-30 parts of nano pigment, 6-10 parts of functional auxiliary agent and 10-20 parts of mixed solvent. The glaze-like coating can form a glaze-like effect without calcination, can ensure the ultrahigh strength, high scratch resistance and high wear resistance of the coating, and has excellent outdoor weather resistance. The coating can be directly matched with epoxy anti-rust primer, electrophoretic primer, powder coating, acrylic paint and other anti-rust paint or various primer coats to form complete coating, and can be applied to outdoor infrastructures needing high hardness and high weather resistance requirements, such as flower pots, flower stands, chairs, animal sculptures and the like, on two sides of urban roads, such as telegraph poles, guard rails, light poles, traffic signal lamps, power distribution cabinets, garbage cans and the like. |
priorityDate | 2017-11-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 61.