http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108117835-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-388 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D163-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-388 |
filingDate | 2018-02-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-01-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108117835-B |
titleOfInvention | A kind of chrome-free fingerprint-resistant environmental protection paint and preparation method thereof |
abstract | The invention discloses a chromium-free anti-fingerprint environmental protection coating, which is composed of the following components in parts by weight: 40-50 parts of a film-forming polycondensate, 5-8 parts of aminopropanol ascorbyl phosphate modified graphene oxide, epoxy resin 15-20 parts of resin, 1-4 parts of dispersant, 1-4 parts of leveling agent, 1-4 parts of defoamer, and 20-40 parts of water. The invention also discloses the preparation method of the chromium-free fingerprint-resistant environmental protection paint, which includes the following steps: adding the film-forming polycondensate into water, stirring evenly, adding other components in proportion, and then adding the film-forming polycondensate to the water at a rate of 800-1300 rpm. Stir and disperse for 50-60 minutes, stir and filter to obtain the finished product. The chromium-free fingerprint-resistant environmental protection paint disclosed by the invention has more excellent corrosion resistance, stability and alkali blackening resistance, and is safe and environmentally friendly to use. |