http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108097327-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_72e6ffa4858f7457fdd0d311a99edb47 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2531-26 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J31-1691 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J31-26 |
filingDate | 2016-11-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7976a3cccf619333bbec7fe030ab8b51 |
publicationDate | 2018-06-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108097327-A |
titleOfInvention | The preparation of galapectite modified composite material |
abstract | The present invention relates to the preparation of galapectite modified composite material, including:It weighs 3.0g galapectites, adds in 75 90mL absolute ethyl alcohols, 3 5g deionized waters after 80 DEG C of 1 3h of reflux, add in 3.0gKH 570, after reaction for 24 hours, washs 3 times with absolute ethyl alcohol, 80 DEG C of dryings, you can obtain the galapectite for being grafted double bond;Weigh 1.25g Zn (NO 3 ) 2 ·6H 2 O, 0.25g amino terephthalic acid (TPA) are dissolved in 33mLDMF, 0.1g, 0.25g and 0.5g carboxylated galapectite, and by transfer reaction kettle after gained suspension ultrasound 20min, 100 DEG C stand 34h.It is collected by centrifugation, 60 80 DEG C of 24 36h of drying, IRMOF 3/COOH HNT composite materials is made. |