http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108084329-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F218-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2-26 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F218-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 |
filingDate | 2017-12-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-12-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108084329-B |
titleOfInvention | Vinegar-acrylic emulsion with high solid content and low viscosity and preparation method thereof |
abstract | The invention belongs to the technical field of vinegar-acrylic emulsion, and discloses a vinegar-acrylic emulsion with high solid content and low viscosity and a preparation method thereof. The preparation method comprises the following steps: adding butyl acrylate, vinyl acetate, isooctyl acrylate, functional monomer and emulsifier into water, stirring and emulsifying uniformly to obtain pre-emulsion; mixing part of butyl acrylate, vinyl acetate, isooctyl acrylate and functional monomers to obtain mixed monomers; preparing inorganic peroxide initiator into solution. Mixing water, an emulsifier, a protective colloid, a buffering agent, a functional monomer and a mixed monomer, stirring and emulsifying, and heating to 75-85 ℃; dripping initiator solution, stirring and polymerizing to obtain seed emulsion; sequentially dropwise adding the pre-emulsion and the rest of the mixed monomers, continuously dropwise adding an initiator solution, and reacting at 80-90 ℃ for 0.5-1 h; and (3) cooling, adding a redox initiator, stirring for 20-60 minutes, stirring, cooling, and discharging to obtain the vinegar-acrylic emulsion with high solid content and low viscosity. |