abstract |
A kind of wear-resistant coating in punching of the rotor of motor is related to motor processing technical field, it is characterised in that:It is made up of the following materials in parts by weight, 11 17 parts of resin, 12 6 10 parts of nylon, modified 6 11 parts of fluorite, 15 parts of carboxymethyl cellulose, 14 parts of starch paste, 14 parts of bamboo charcoal, 26 parts of Cocoamidopropyl betaine, 26 parts of 2 hydroxy propyl ester of acrylic acid, 26 parts of dihydromethyl propionic acid, 15 parts of dibutyl phthalate, 37 parts of termil, 37 parts of pentaerythritol triacrylate, 8 15 parts of antifoaming agent, 8 15 parts of anti-aging agent, 5 10 parts of biomass auxiliary material, 20 27 parts of deionized water.The method of the present invention is reasonable, easy to operate, wear-resisting, corrosion-resistant. |