http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108070282-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2de94c5627848834f3db092e89b6b3a8 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21D1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23C8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21D9-0068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21D1-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C21D1-74 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D4-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D1-74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D1-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C21D1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C23C8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D1-00 |
filingDate | 2017-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_972cabb104e4c6ff175b617417e42f53 |
publicationDate | 2018-05-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-108070282-A |
titleOfInvention | A kind of high-strength, antioxidant metallic vehicle door handle and its Surface heat-treatent modified technique |
abstract | The invention discloses a kind of high-strength, antioxidant metallic vehicle door handles, and including handle body, high intensity layer is pressed coated with a floor height intensity anti oxidation layer, high-strength, antioxidant layer outside handle body:Anti oxidation layer=3:2 ratio mixing, ingredient include following components according to the mass fraction:High intensity layer includes following components according to the mass fraction:1 butanol:11 19 parts, polypropylene carbonate fat:28 parts, pigment:10 14 parts, filler:9 13 parts, black silicon carbide:12 17 parts, fine-grained alumina:20 23 parts, molybdenum disulfide:38 parts, zinc oxide:18 parts, ionic liquid blast reducer:11 19 parts, curing agent:7 11 parts, delustering agent:12 18 parts;Anti oxidation layer includes following components according to the mass fraction:Base-material lotion:12 19 parts, antifreezing agent:20 22 parts, polyphenylene oxide resin powder:21 18 parts, butadiene-styrene rubber:11 18 parts, styrene:48 parts, trichloro ethylene:6 11 parts, toluene:11 13 parts, plasticizer:11 19 parts, coupling agent:20 26 parts, auxiliary material:28 parts. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109023085-A |
priorityDate | 2017-12-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 96.