http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-108035145-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d0a3456a6b2c313a61c072e9180a21e6
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F8-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F1-10
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D06M13-005
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F8-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D06M13-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-34
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10
filingDate 2017-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_394031dc52dc77f488764c442990dad8
publicationDate 2018-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-108035145-A
titleOfInvention A kind of production method of fragrance fabric with soft bags
abstract The invention belongs to technical field of textile fabric, and in particular to a kind of production method of fragrance fabric with soft bags, including following production stage, a. prepare fragrant fiber:Using composite spinning method, by spices and spinning material melt spinning, perfume molecules are melted in ultra-fine fibrous inside, obtain fragrant fiber, the spices mixes after being refined by the flower such as rose, jasmine, green tea and tulip;B. Aroma fabric arranges:Aroma fabric is arranged using padding method or infusion process, padding method:Working solution is padded in preparation, is firstly added the spices of 20g/L, the water that amount temperature is 40 DEG C 70 DEG C such as adds, after spices is mixed and stirred for into uniform thin pulp with water, adds remaining water, add the SCJ 939 of 20g/L, be uniformly mixing to obtain and pad working solution;After Aroma fabric is padded with pick-up rate 70 80% using above-mentioned gained working solution, the Aroma fabric drying after being padded with 80 DEG C 100 DEG C, obtains fragrance fabric with soft bags.
isCitedBy http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109295709-A
priorityDate 2017-12-29-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962

Total number of triples: 20.