http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107887596-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c4444deff2c18957d58415d895c2913d |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-5825 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-505 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-485 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-58 |
filingDate | 2017-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df3c3625bb762647becad00e54bdd4c7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e2e55ad2467cbc5e7d7bbb6e3e3ee8be http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3e0b3a3d2d436b4e386bc34face35919 |
publicationDate | 2018-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107887596-A |
titleOfInvention | A kind of manganate cathode material for lithium preparation method |
abstract | The present invention provides a kind of manganate cathode material for lithium preparation method, comprises the following steps:1) carbon microbeadses are added in deionized water, ultrasonic disperse uniformly forms the carbon microbeadses suspension that concentration is 0.5 2g/L afterwards;Potassium permanganate is added in deionized water, stirs to after being completely dissolved the liquor potassic permanganate for forming that concentration is 100 700g/L;2) by the carbon microbeadses suspension and the liquor potassic permanganate according to Mn:C=2.1 2.8 molar ratio mixing, stirring reaction are centrifuged and obtain centrifugation product afterwards for a period of time;3) manganese dioxide presoma will be obtained after the centrifugation product washing, drying;4) by the manganese dioxide presoma and lithium salts according to Li:Mn=0.45 0.65 molar ratio is scattered in water or alcohol solvent, and the mixture obtained after drying calcines 8 24h at a temperature of 500 900 DEG C, and manganate cathode material for lithium can be obtained after cooling. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-114394624-A |
priorityDate | 2017-09-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.