http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107880688-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0d94cb3f19078e3507ad359c2657da7a |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2227 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D143-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-33 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00 |
filingDate | 2017-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34f00a34a52f86db8bbf507bbf82685a |
publicationDate | 2018-04-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107880688-A |
titleOfInvention | A kind of third compound heat-insulating energy-saving paint of silicon of high-decoration energy and preparation method thereof |
abstract | The present invention provides a kind of the third compound heat-insulating energy-saving paint of silicon of high-decoration energy, and its raw material includes following components by weight:50 60 parts of silicone acrylic emulsion, 5 10 parts of covering emulsion, 25 parts of hollow glass bead, 8 15 parts of diatomite, 5 10 parts of nano titanium oxide, 6 10 parts of heat-reflecting heat-insulating powder, 5 10 parts of alumina powder, 36 parts of mica powder, 38 parts of titanium dioxide, 0.3 0.6 parts of antimildew disinfectant, 95 0.3 0.9 parts of AMP, 0.5 1.0 parts of dispersant, 0.2 0.5 parts of defoamer, 1.0 2.5 parts of coalescents, 0.5 0.8 parts of thickener, 0.1 0.3 parts of wetting agent, 30 50 parts of deionized water.The present invention also provides its preparation method, the coating not only has good freeze-thaw stability, water resistance, alkali resistance, abrasion resistance, weather resisteant, polluting proofing property and an ageing resistance, but also the advantages such as coating temperature-change resistance, compound heat-insulation, environmental protection and energy saving, high-decoration, thermal conductivity factor be low. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112080179-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112745730-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112143312-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112663394-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-115286965-A |
priorityDate | 2017-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 53.