http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107845447-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-066 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2207-062 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2203-202 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02A30-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B7-292 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01B11-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01B7-29 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 |
filingDate | 2017-09-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107845447-B |
titleOfInvention | Low-attenuation capacity-expanding photoelectric composite low-voltage cable |
abstract | The invention discloses a low-attenuation capacity-expanding photoelectric composite low-voltage cable, wherein insulating layers are coated on the outer surfaces of a ground core conductor, 3 power core conductors and a control core conductor, a first heat-resistant sheath layer is coated on the outer surface of a photoelectric unit, and a reserved optical channel consists of a tensile insulating layer and a second heat-resistant sheath layer coated on the outer surface of the tensile insulating layer; the first heat-resistant sheath layer and the second heat-resistant sheath layer are composed of the following components: high-density polyethylene resin, low-density polyethylene resin, poly-p-benzamide, trioctyl trimellitate, stearic acid, barium stearate, tributyl citrate, diatomite, maleic anhydride grafted PE, calcium-zinc heat stabilizer, antioxidant and aminopropyltriethoxysilane. The aging test temperature of the thermoplastic sheath material reaches 158 ℃, and the change rate of the tensile strength and the change rate of the elongation at break are not more than +/-20%. |