http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107840772-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06D5-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B31-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B31-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B31-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06D5-06 |
filingDate | 2017-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107840772-B |
titleOfInvention | High-burning-rate gas generating agent and granulating process thereof |
abstract | A high-burning-rate gas generating agent and a granulation process thereof are disclosed, guanidine nitrate, basic copper nitrate, an auxiliary agent and water are added into a container, the container is heated, the temperature is controlled to be 70-90 ℃, then dispersing equipment is used for stirring and dispersing to obtain a uniformly mixed material, a spraying equipment is used for drying the material to obtain dried particles 1, the particles 1 are sized to obtain particles 2, and the particles 2 are dried to obtain particles 3; the granules 3 are compressed into tablets. The invention has higher burning rate and can meet the performance requirements of generators with special requirements on speed, such as side airbags and the like. The process can reduce the cost of raw materials, so that the raw materials do not need to be dried and crushed before use, the components can be ensured to be fully contacted and mixed, and the stability and consistency of the product are improved; the soluble raw materials are completely dissolved by using a heating and dissolving mode, and the undried wet basic copper nitrate and a basket type sand mill are used for grinding and dispersing to obtain uniform materials, so that the operation is convenient, and the production efficiency is higher. |
priorityDate | 2017-03-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |