http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107793559-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_77551c93f60bd12e621993c0e6b4e32e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D167-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D167-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-49 |
filingDate | 2016-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9f3701cc819a958f09931945f0cc6813 |
publicationDate | 2018-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107793559-A |
titleOfInvention | A kind of preparation method of low-temperature quick-dry alkyd resin |
abstract | The invention discloses a kind of low-temperature quick-dry alkyd resin, is used with linolenic acid, behenic acid, benzoic acid, tung oil collocation, then is added pentaerythrite, trimethylolpropane, phthalic anhydride, triphenyl phosphite, hypophosphorous acid, dimethylbenzene and 200#.This resin-made obtains the advantages that varnish dryness is fast, hardness is high, paint film richness is good, guarantor's light colour retention is all good. |
priorityDate | 2016-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |