http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107754819-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-049 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-047 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-1004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-725 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-34 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-047 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-72 |
filingDate | 2017-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-11-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107754819-B |
titleOfInvention | Synthesis of photocatalyst SnS with visible light response2/Bi2WO6Preparation method of nanosheet |
abstract | Synthesis of photocatalyst SnS with visible light response 2 /Bi 2 WO 6 The preparation method of the nano-sheet comprises the step of preparing Bi by a hydrothermal method 2 WO 6 Then SnCl is added 4 ·5H 2 Dissolving O in the mixed solution of acetic acid and ethanol, and then adding Bi 2 WO 6 Carrying out ultrasonic treatment, adding thioacetamide to obtain a mixed solution after the treatment is finished, stirring the mixed solution at room temperature for 5 hours, putting the mixed solution into a high-temperature reaction kettle, reacting the mixed solution at 120-220 ℃ for 8-16 hours, naturally cooling the mixed solution to the room temperature, filtering, washing and drying a product after the reaction is finished to finally obtain SnS 2 /Bi 2 WO 6 . Invention SnS 2 /Bi 2 WO 6 The specific surface area is large, and the adsorption capacity is strong; the visible light absorption performance is better, and the photocatalytic oxidation degradation of organic pollutants is greatly improved; furthermore, the invention SnS 2 /Bi 2 WO 6 The preparation method is simple and easy to operate. |
priorityDate | 2017-11-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |