http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107684914-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2523-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-40 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8876 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-0033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-088 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-38 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-887 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-10 |
filingDate | 2017-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107684914-B |
titleOfInvention | Magnetic Bi2MoO6/CuFe2O4Composite photocatalytic material and preparation method thereof |
abstract | The invention discloses a magnetic Bi 2 MoO 6 /CuFe 2 O 4 The composite photocatalytic material and the preparation method thereof are as follows: adding Bi 2 MoO 6 Ultrasonically dispersing in deionized water, and adding Cu (NO) 3 ) 2 ·3H 2 O、Fe(NO 3 ) 3 ·9H 2 Placing O and disodium ethylene diamine tetraacetate in a water bath at 20-30 ℃ and stirring for 0.5-1 h to obtain a suspension A, adding urea to the suspension A, placing the suspension A in a water bath at 50-80 ℃ to react for 0.5-2 h to obtain a mixed suspension B, placing the mixed suspension B in a hydrothermal reaction kettle at 120-160 ℃, stirring to react for 1-8 h, filtering, washing and drying the obtained reaction mixed solution to obtain a solid, placing the solid in a muffle furnace to calcine at 400-700 ℃ for 1-3 h to obtain magnetic Bi with high catalytic activity 2 MoO 6 /CuFe 2 O 4 A composite photocatalytic material. The invention overcomes the defect of Bi 2 MoO 6 Has the defects of easy recombination of electron holes and poor recoverability, and prepares the magnetic Bi 2 MoO 6 /CuFe 2 O 4 The process of the composite photocatalytic material has the advantages of high efficiency and easy operation, and can replace TiO 2 And ZnO and the like are applied to photocatalytic purification of printing and dyeing wastewater, medical wastewater and heavy metal wastewater. |