http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107629329-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2a97b9db01766f4cb68654535207c24a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L77-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-098 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-09 |
filingDate | 2016-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_41d5cbc42528f1acb07fffe6d7668b80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9264cd52814d954b392a75ddd08cacf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_642782c2410cff6cc84f1866469dda6e |
publicationDate | 2018-01-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107629329-A |
titleOfInvention | High temperature and tear resistant conveyor belt |
abstract | The invention discloses a high-temperature-resistant and tear-resistant conveyor belt. The components of the raw materials are composed as follows in parts by weight: 100 parts of composite masterbatch, 5-7 parts of chlorosulfonated polyethylene with a chlorine content of 25-30%, and 6-6 parts of carbon black 8 parts, 10-15 parts of glass fiber, 10-12 parts of aramid staple fiber, 2-4 parts of N-(4-anilinophenyl) maleimide, 0.6-0.8 parts of zinc dimethacrylate, 6-8 parts of mixed resin, 1-2 parts of adhesive, 6-8 parts of reinforcing filler, 2-4 parts of vulcanizing agent, 2-3 parts of stearic acid, 1.2-1.5 parts of anionic surfactant, Coke agent CTP 0.6-0.8 parts, pine tar oil 2-4 parts, anti-aging agent AW 1.5-1.8 parts. The invention enables the conveyor belt to have the effects of high strength and high tear resistance, significantly reduces the rolling resistance and dynamic heat generation of the rubber material, improves the properties of the rubber material of the conveyor belt such as cutting resistance, flex fatigue resistance, and crack growth resistance, and at the same time can It has a very good bonding transition effect on the rubber material of the high heat resistant conveyor belt, prevents delamination, improves the thermal stability of the rubber material, and is beneficial to prolong the service life of the conveyor belt. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109292363-A |
priorityDate | 2016-07-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 51.