titleOfInvention | Method for synthesizing tin selenide microcrystalline powder by hydrothermal method |
abstract | A method for synthesizing tin selenide micron crystal powder by a hydrothermal method comprises the steps of dissolving tartaric acid in distilled water, adding tin dichloride, stirring until the solution is clear and transparent to prepare a solution A, sequentially adding selenium dioxide, sodium hydroxide and sodium borohydride into the distilled water to prepare a solution B, slowly adding the solution A into the solution B, reacting for 6-24 hours at 180 ℃ in a hydrothermal reaction kettle, centrifuging, washing and drying to obtain tin selenide black powder. |