http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107565119-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 |
filingDate | 2016-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-01-01-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107565119-B |
titleOfInvention | Negative electrode active material, preparation method thereof and lithium ion battery |
abstract | The invention relates to a rod-shaped lithium molybdate cathode active material, wherein the rod-shaped lithium molybdate is of a micron-sized rod-shaped structure; the diameter of the rod-shaped lithium molybdate is 1-2 mu m; the length is 1-7 μm. The invention also provides a preparation method of the rod-shaped lithium molybdate cathode active material and a lithium ion battery. According to the invention, the micron-sized rod-shaped lithium molybdate is used as the negative active material, the particle size is smaller, the de-intercalation of lithium ions is facilitated, meanwhile, the solid structure is beneficial to reducing the specific surface area of the material, reducing side reactions and improving the compaction density and the volume specific capacity of the material, and the preparation process is simple. |
priorityDate | 2016-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links