http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107541052-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f71b5786264a03b20f7b83472a361778 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-1515 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L75-04 |
filingDate | 2017-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_51e1d4d82c7abeb46b9205c3abe9774a |
publicationDate | 2018-01-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107541052-A |
titleOfInvention | A kind of anlistatig polyurethane elastomer |
abstract | The invention discloses a kind of anlistatig polyurethane elastomer, it by weight than being made up of 100/65 component A and component B, the raw material of the component A by following percentage by weight material composition:Sodium methyl silicate 60 70%, palmitic acid 20% 38%, phytosterol 1 2%, wherein, phytosterol is γ aminopropyl triethoxysilanes in the component A;The raw material of the component B by following percentage by weight material composition:Sodium methyl silicate 61 85%, polytetrafluoroethylene (PTFE) 12 35%, catalyst 0.05% 1%, age resister 0.8%, antistatic additive 4%, polytetrafluoroethylene (PTFE) is diethyl toluene diamine in the component B;Catalyst is lauric acid diethyl amide in the component B;Age resister is the phosphoamide of saturation 18 in the component B;Antistatic additive is expoxy propane in the component B, and the anlistatig polyurethane elastomer that the present invention obtains, not only physical and mechanical properties is superior, and product surface resistance can reach 107 8 Ω, and volume resistance can reach 106 7 Ω, and antistatic property is superior. |
priorityDate | 2017-09-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |