http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107502227-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2433-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2303-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2429-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2312-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2439-06 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J3-246 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J103-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08B31-12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B31-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J103-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-06 |
filingDate | 2017-08-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107502227-B |
titleOfInvention | A kind of non-ionic starch based adhesive and preparation method thereof |
abstract | The present invention provides a kind of non-ionic starch based adhesive and preparation method thereof, and the preparation method successively includes pre-treatment step, hydroxypropyl etherified step, crosslinking treatment step, wherein hydroxypropyl etherified step and the sequence of crosslinking treatment step can exchange;The pre-treatment step includes that starch is deployed into starch milk with alcohol;The hydroxypropyl etherified step includes that alkaline reagent and propylene oxide are added into the product of previous step, is heated to 50-80 DEG C of reaction 6-12h;The crosslinking treatment step includes that crosslinking agent and modifying agent are added into the product of previous step, and the pH value for controlling reaction system is 10-11, reacts 2-6h at 40-70 DEG C of temperature;The modifying agent is at least one of polyvinyl alcohol, polyvinylpyrrolidone, polyacrylamide.Non-ionic starch based adhesive provided by the invention can be applied in the putty or mortar of a variety of base-materials such as cement, gypsum, grey calcium, have good cold water-soluble, higher viscosity and acid and alkali-resistance, salt stability. |