http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107408462-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B2204-22 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B32-23 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B05D3-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01G11-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-28 |
filingDate | 2016-02-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107408462-B |
titleOfInvention | Method for depositing oxidized carbon-based microparticles and nanoparticles |
abstract | The invention relates to the field of elements for storing energy and to a method for depositing nano/microparticles comprising at least graphene sheets on a support (8), said method comprising the following steps: at least graphene oxide sheets; suspending the nano/micro particles in at least one solution, the solution comprising at least water as a solvent; spraying each suspension on a substrate (15) by means of hydrodynamic instability; heating the substrate (15) during each spray to a temperature less than or equal to one and one half times the boiling point of each of the aforementioned solutions and less than or equal to 200 ℃ so as to promote complete evaporation of the solvent from each portion of each suspension sprayed on the substrate (15); after spraying, the deposit (1) is reheated to a temperature sufficient to at least deoxygenate the oxidized graphene present in the deposit (1) and greater than the temperature of the substrate (15) during the deposition step. |
priorityDate | 2015-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |