http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107400435-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C07C231-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C23F11-173 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C231-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07C233-20 |
filingDate | 2016-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-08-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107400435-B |
titleOfInvention | A kind of esters of acrylic acid corrosion-inhibiting coating liquid and its preparation method and application that can be automatically repaired in sodium-chloride water solution |
abstract | The invention discloses the esters of acrylic acid corrosion-inhibiting coating liquid and its preparation method and application that one kind can be automatically repaired in sodium-chloride water solution, belong to corrosion of metal protection field.Coating solution of the present invention is made of the terpolymer and solvent that n-butyl acrylate, n-BMA and dopamine Methacrylamide are obtained by copolyreaction, wherein, n-butyl acrylate, n-BMA, three kinds of monomers of dopamine Methacrylamide molar ratio be 3~6:2~6:1~2.A kind of corrosion-inhibiting coating liquid of the invention, mainly for the preparation of the erosion shield of metal or nonmetallic materials in salt water.Experiments have shown that, acrylate type coating of the invention can the self-regeneration in 5% sodium-chloride water solution, have many advantages, such as that matrix adhesive force is big, anticorrosive property is excellent and good decorative property simultaneously, and moulding process is easy, technical requirements are low, is suitable for preparing the surface covering of the materials such as various organic (various resins), inorganic (ceramics, glass), metal. |
priorityDate | 2016-05-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 72.