http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107359321-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-625 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-628 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-624 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-0525 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y30-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M10-0525 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M4-38 |
filingDate | 2017-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107359321-B |
titleOfInvention | The lithium sulfur battery anode material and preparation method thereof of the nitrogen-doped carbon of spherical structure/titanium oxide bivalve cladding titanium oxide/sulphur |
abstract | A kind of lithium sulfur battery anode material of the nitrogen-doped carbon of spherical structure/titanium oxide bivalve cladding titanium oxide/sulphur:The outer spherical shells of NC coat Ti 4 O 7 Interior spherical shell contains Ti in interior spherical shell 4 O 7 Nano particle (3) and nano-sulfur (4);Preparation method:S1, by SiO 2 Microballoon, which is dispersed in organic solution, carries out liquid phase coating, is calcined being put into Muffle furnace after products therefrom conventional filtration, cleaning;Products therefrom is carried out liquid phase nitrogen containing monomer polymerization cladding, conventional filtration, cleaning and vacuum drying by S2;Products therefrom is carried out high temperature cabonization and reduction treatment, products therefrom is distributed in alkaline solution and is performed etching, and is ultrasonically treated by S3, after conventional filtration, cleaning, is carried out vacuum drying treatment, is obtained composite material;Products therefrom is distributed in the aqueous solution containing sulfosalt by S4, then dilute weak acid solution is added dropwise and stirs, and is put into inert gas filled closed container after conventional filtration, cleaning and vacuum drying, slowly up to composite material after heating, constant temperature. |
priorityDate | 2017-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |