http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107266972-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-107 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-03 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-033 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-107 |
filingDate | 2017-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2020-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2020-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107266972-B |
titleOfInvention | Thermosetting type hollow coated glass protection ink and preparation method thereof |
abstract | The invention provides thermosetting type hollow coated glass protection ink and a preparation method thereof, wherein the protection ink comprises the following components in parts by mass: 45-50 parts of thermosetting acrylic resin, 45-55 parts of solvent, 10-30 parts of filler and 2-5 parts of auxiliary agent. The protective ink has good screen printing performance and fine lines, and has no edge leakage and no burr after being amplified by 100 times in two dimensions; the drying speed is high, the scratch resistance is high, and the protection performance is good; the ultrasonic cleaning resistance is good, the film stripping time is short, and no residue is left after cleaning. The preparation method is simple in process and suitable for industrial production. |
priorityDate | 2017-07-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |