http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107216764-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac6685527a991f9d857c1a4af55d1968 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-282 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-1804 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3834 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-3893 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F220-18 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-25 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-08 |
filingDate | 2017-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f6b32f00405c70f9c2b994230cd0910f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a88c999acfabddab9b52e05fdec1c90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92e54c1bce8edafb54ef97fb8a4f12ce |
publicationDate | 2017-09-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107216764-A |
titleOfInvention | A kind of preparation method of the environmentally friendly coatings of non-orientation silicon steel |
abstract | The invention belongs to non-orientation silicon steel production technical field, and in particular to a kind of preparation method of the environmentally friendly coatings of non-orientation silicon steel.The present invention butyl acrylate and ethyl acetate are incubated under nitrogen protection after with acrylic acid, Isooctyl acrylate monomer etc. is mixed, adipic dihydrazide is added dropwise while stirring, toluene di-isocyanate(TDI) is added after heating, ethanedioic acid etc. and the mixture for adding methylvinyldichlorosilane and triethylene diamine mixing, stirring is distilled after standing, adjust and the environmentally friendly coatings base fluid of non-orientation silicon steel is obtained after pH, then by titanium dioxide, crushed after the melting of the ball millings such as silica, and mix with the environmentally friendly coatings base fluid of non-orientation silicon steel etc. and can obtain non-orientation silicon steel environmental protection coatings, the environmentally friendly coatings of non-orientation silicon steel prepared by the present invention efficiently solve the coatings poor heat resistance used at present, the problem of stability and poor covering power, high annealing is difficult dry linting, coating hardness is high, creep is not susceptible to after heated. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111619257-A |
priorityDate | 2017-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 71.