http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107201166-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-03 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1675 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-1687 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-16 |
filingDate | 2017-05-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107201166-B |
titleOfInvention | A kind of macromolecule surface protective coating and preparation method thereof |
abstract | The present invention provides a kind of macromolecule surface protective coatings and preparation method thereof.Wherein, which comprises by weight, in 720 parts of water, 100 parts of macromolecule methyl-silicone oils, 3 parts of emulsifiers and 0.5 portion of protective agent is added, 85 ° to 95 ° at a temperature of, with the first mixing speed, stirring and emulsifying obtains first lotion;By weight, in 720 parts of water, 100 parts of macromolecule amido silicon oils and 3 parts of emulsifiers are added, 75 ° to 85 ° at a temperature of, with the second mixing speed, stirring and emulsifying obtains second lotion;By predetermined ratio, first lotion and second lotion is added, stirs and obtains the macromolecule surface protective coating after filtering. |