http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107163856-A

Outgoing Links

Predicate Object
assignee http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_79c2b828b2090853d62615ba81d8d324
classificationCPCAdditional http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-265
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-2241
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-16
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-05
classificationCPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D201-00
classificationIPCInventive http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D197-02
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D201-00
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D5-14
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-04
filingDate 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
inventor http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_057c85a97c31070a3360a37d95c2305f
publicationDate 2017-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date>
publicationNumber CN-107163856-A
titleOfInvention A kind of preparation method of coating for wall surface
abstract The invention discloses a kind of preparation method of coating for wall surface, with following composition by weight than raw material be conventionally made, raw material is:250 400 parts of water, 35 parts of alkaloid, 35 parts of defoamer, 80 150 parts of stibium trioxide powder, 35 parts of wetting agent, 50 80 parts of talcum powder, 100 180 parts of oyster shell whiting, 30 60 parts of bamboo pulp, 100 180 parts of synthetic resin emulsion, 35 parts of insect prevention bacteriostatic agent, 35 parts of preservative, 30 60 parts of methyl-silicone oil.It is a large amount of in the coating of the present invention to use plant, biomaterial, harmful substance is not contained in these materials, so as to improve the environmental-protecting performance of coating, be conducive to health, the antibacterial effect of insect prevention can also be played simultaneously, give people to provide beneficial comfortable living environment, when water is splashed on metope, dope layer will not absorb moisture, avoid wall coating from foaming after absorbing water to split away off, when the pollutants such as grease, prepared Chinese ink are coated with wall, metope can be kept clean pollutant wiped clean using rag.
priorityDate 2017-05-24-04:00^^<http://www.w3.org/2001/XMLSchema#date>
type http://data.epo.org/linked-data/def/patent/Publication

Incoming Links

Predicate Subject
isDiscussedBy http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID8058
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID458393636
http://rdf.ncbi.nlm.nih.gov/pubchem/taxonomy/TAXID292582
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID292582
http://rdf.ncbi.nlm.nih.gov/pubchem/anatomy/ANATOMYID8058
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID5354495
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419549163
http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID962
http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID419512635

Total number of triples: 28.