http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107163680-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_223c4cebeb338bbc63006872b80101c3 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-104 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-107 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D11-106 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-107 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-106 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-104 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-03 |
filingDate | 2017-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6285efde198cc53265f1abec0e36d6a5 |
publicationDate | 2017-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107163680-A |
titleOfInvention | A kind of water-based ink of ad production and preparation method thereof |
abstract | The invention discloses a kind of water-based ink of ad production, it is characterised in that includes following raw material according to parts by weight:10 ~ 20 parts of acrylic resin, 2 ~ 10 parts of isopropanol, 3 ~ 10 parts of dimethylbenzene, 2 ~ 18 parts of pigment, 5 ~ 15 parts of white hydrogenated petroleum resin, 10 ~ 15 parts of polypropylene glycol adipate, 5 ~ 10 parts of dipropylene glycol dibenzoate, 2 ~ 8 parts of kiwi fruit acid esters, 3 ~ 9 parts of alkyd resin, 2 ~ 10 parts of wetting agent, 3 ~ 10 parts of dispersant, 1.5 ~ 3.5 parts of defoamer, 2 ~ 10 parts of levelling agent, 2.5 ~ 6.5 parts of anion surfactant.The present invention provides a kind of water-based ink of ad production and preparation method thereof, obtained water-based ink moderate drying speed, avoid because ink setting speed causes to cause dry plate soon, the dried slow phenomenon for causing printed matter surface ink film to shrink is prevented again, and the viscosity of water-based ink is low, glossiness is high, low manufacture cost, both with actual application value. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-113637207-A |
priorityDate | 2017-07-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 58.