http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107159257-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac8dae81dbbe9cce62c6b20a40a349e4 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-084 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-343 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-28054 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J20-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8946 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J37-10 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-89 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J37-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J20-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J35-10 |
filingDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfc353011c6d768423dc4470d6c7de0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f204efb5fc2df53b89f8a8051d3dda14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e9eea5deb080cc822437b3e0bb8591cf |
publicationDate | 2017-09-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107159257-A |
titleOfInvention | The preparation method of ozone Heterogeneous oxidation solid catalyst |
abstract | The present invention relates to a kind of preparation method of ozone Heterogeneous oxidation solid catalyst, category environmental protection and technical field of chemical engineering catalysts.With medical stone, wollastonite, activated carbon, carnallite, illite and raphite make carrier, carrier is modified through lithium hypochlorite and double (acetylacetone,2,4-pentanedione) beryllium reamings, add surfactant myristyl tributyl ammonium chloride and surface activation process is carried out under ul-trasonic irradiation, then activated carrier in hydrothermal reaction kettle with composite mineralizer borax and potassium sulfate, catalytic activity auxiliary agent predecessor isopropyl scandium oxide (III), three (4, 4, (2 thiophene) 1 of 4 trifluoro 1, 3 diacetyl) europium, three (2, 2, 6, 6 tetramethyls 3, 5 heptadione acid) gadolinium, ten water holmium oxalates, catalytic active center component predecessor titanocenes ring substituted salicylic acid complex, cupric glutamate, chlordene osmium dipotassium, the ammino platinum of dichloro two, hydro-thermal reaction is carried out under the effect of emulsifying agent didodecyldimethylammbromide bromide, drying removes moisture, calcination obtains ozone Heterogeneous oxidation solid catalyst in Muffle furnace. |
priorityDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |