http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107058720-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-243 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-2406 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B1-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B1-243 |
filingDate | 2017-04-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-12-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107058720-B |
titleOfInvention | A method of cementite is prepared using low-grade complex iron ore |
abstract | The present invention discloses a kind of method using low-grade complex iron ore preparation cementite, comprising: is uniformly mixed low-grade complex iron ore with binder, and pelletizing material is made;The pelletizing material is made into green-ball and is roasted after drying, carburizing pelletizing is obtained;By the carburizing pelletizing in CO+CO 2 +H 2 Or CH 4 +H 2 Carburizing, cooling in inert atmosphere is carried out in gas, obtains pelletizing after carburizing;Pelletizing after the carburizing is subjected to wet ball-milling, wet magnetic separation is carried out after ball milling, is dried to obtain cementite.Method provided by the invention prepares cementite efficient quick, low in cost, energy conservation and environmental protection. |