http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-107051493-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ac8dae81dbbe9cce62c6b20a40a349e4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2101-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2523-00 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-281 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-898 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-725 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-30 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-78 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J32-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-89 |
filingDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_99ab4dee9b6f673fd03589358ae43e72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dfc353011c6d768423dc4470d6c7de0c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f204efb5fc2df53b89f8a8051d3dda14 |
publicationDate | 2017-08-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-107051493-A |
titleOfInvention | The preparation method of ozone Heterogeneous oxidation solid catalyst |
abstract | The present invention relates to a kind of preparation method of ozone Heterogeneous oxidation solid catalyst, category environmental protection and technical field of chemical engineering catalysts.The preparation method is pure with diatom, kyanite, cubric niter, dolomite, amazonite and lithium lime stone porous material make carrier, carrier is modified through lithium hypochlorite and double (acetylacetone,2,4-pentanedione) beryllium reamings, add surfactant Cationic surfucant and surface activation process is carried out under ul-trasonic irradiation, then ultrasonic surface activated carrier in hydrothermal reaction kettle with composite mineralizer borax and potassium sulfate, catalytic activity auxiliary agent predecessor three (hexafluoroacetylacetone) yttrium (III) dihydrate, acetylacetone,2,4-pentanedione samarium, three (4, 4, (2 thiophene) 1 of 4 trifluoro 1, 3 diacetyl) europium, ten water holmium oxalate Rare-earth chemicals, catalytic active center component predecessor normal transition metallo-organic compound pyruvic acid isonicotinoyl hydrazone vanadium, citric acid nickel, cupric glutamate and the hydration iridium of precious metal chemical complex tetrachloro two, hydro-thermal reaction is carried out under the effect of the hydroxypropyl dichloride ammonium of emulsifying agent N dodecyl dimethyl N ' trimethyls 2, reaction product drying is removed after moisture, in Muffle furnace, calcination obtains ozone Heterogeneous oxidation solid catalyst under certain temperature. |
priorityDate | 2017-04-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links