http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106975485-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W10-37 |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F101-22 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-652 |
filingDate | 2017-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-07-02-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106975485-B |
titleOfInvention | The catalyst and its preparation method and application of Cr (VI) in a kind of Efficient Conversion water |
abstract | The present invention relates to the catalyst and its preparation method and application of Cr (VI) in Efficient Conversion water a kind of.By Er 3+ :YAlO 3 It is added Ti (OBu) 4 、Sr(NO 3 ) 2 In NaOH mixed liquor, is reacted under the conditions of 180 DEG C for 24 hours, obtain Er 3+ :YAlO 3 @SrTiO 3 ;By Er 3+ :YAlO 3 @SrTiO 3 It is dissolved in ethyl alcohol, ultrasonic disperse, while HAuCl is added 4 ·4H 2 O solution, after heating under boiling point;2h is calcined at 350 DEG C, obtains Er 3+ :YAlO 3 @(Au/SrTiO 3 )-Au;By Er 3+ :YAlO 3 @(Au/SrTiO 3 )-Au and WO 3 Mixing, ultrasonic disperse will heat 30-40 minutes under suspension boiling point, calcine 2h at 350 DEG C, obtain target product.The method of the present invention is simple and novel, at low cost, and not will cause environmental pollution without by-product generation. |
priorityDate | 2017-04-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |