http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106975100-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L26-0061 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/A61L26-0004 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L26-00 |
filingDate | 2016-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-06-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106975100-B |
titleOfInvention | A kind of nanocomposite and its preparation method and application of cerium oxide/mesoporous silicon |
abstract | The present invention relates to a kind of nanocomposite of cerium oxide/mesoporous silicon, the cerium oxide nanocrystal of cerium oxide nanocrystal and amido modified nanometer particle comprising ligand conversion, ligand conversion is modified in the surface of amido modified nanometer particle;The mass ratio of cerium oxide nanocrystal that ligand is converted and amido modified nanometer particle is 1~20;The cerium oxide nanocrystal of ligand conversion carries out ligand conversion using 2- bromo acid.The invention further relates to the preparation method of cerium oxide/mesoporous silicon nanocomposite and its applications in wound healing or tissue repair.The active oxygen radical that the composite material can balance the surface of a wound is horizontal, reduces level of inflammation, plays adhesive effect using nanometer bridge effect;And preparation reaction system is mild, and condition is controllable, and prepared material all has good biocompatibility, has good clinical conversion possibility. |