abstract |
The embodiment of the invention discloses a MoS x Carbon black nanocomposite, method for the production thereof and use thereof, wherein the MoS x In the carbon black nanocomposite, x is not less than 2 and not more than 2.3, and the MoS is based on the total mass of the nanocomposite x The mass percentage of the component (A) is 5-50%. MoS prepared by the invention x The performance of the/carbon black nanocomposite is comparable to, and even improved by, about 20% over, the commercial 20% Pt/C catalyst. MoS prepared separately x The carbon black nanocomposite also has good catalytic stability, and the catalytic performance of the nanocomposite is not obviously reduced after 5000 catalytic cycles. |