Predicate |
Object |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G2110-0025 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-4018 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C1-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6611 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-6622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09C3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K5-523 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G18-7664 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G101-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-46 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-66 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-76 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G18-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-523 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 |
filingDate |
2017-03-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2019-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate |
2019-10-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
CN-106928491-B |
titleOfInvention |
A kind of microencapsulation expansible graphite and its preparation method and preparing the application in composite polyurethane rigid foam |
abstract |
The present invention relates to a kind of microencapsulation expansible graphites, it is a kind of melamine resin-epoxy resin double-coating expansible graphite, it wraps up melamine microcapsules first i.e. outside expansible graphite, is then enclosed with melamine resin-epoxy resin double-coating expansible graphite microencapsulation expansible graphite of epoxy resin micro-capsule again.It can be used as fire retardant and is used to prepare hard polyurethane foam, and obtained hard polyurethane foam density is 60kgm ‑3 Left and right;Thermal coefficient is 0.03W (mk) ‑1 Left and right;Compressive strength is 0.60MPa or so;Limit oxygen index is close to 30%.The invention discloses its preparation methods. |