http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106884093-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P10-20 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B11-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B9-00 |
filingDate | 2017-03-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-11-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106884093-B |
titleOfInvention | A kind of thick aurin smelting method |
abstract | The present invention relates to a kind of thick aurin smelting methods, and specific step is as follows:(1) thick gold nitric acid solution digestion, is obtained by filtration filter residue I;(2) potassium nitrate is added in filter residue I, is roasted after mixing, obtains fired slags;(3) potassium hydroxide solution digestion is added in fired slags, filter residue II is obtained by filtration;(4) by the nitric acid digestion of filter residue II, filter residue III is obtained by filtration;(5) hydrochloric acid is added in filter residue III and filtrate is obtained by filtration in hydrogen peroxide reaction, handle, obtain bronze.For bronze purity after being refined using this method 99.99% or more, which overcomes the general wet process-disadvantage that pyrogenic process combination product purity is not high, smelting temperature is high, process flow is complicated, the period is long. |