http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106865596-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-64 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-32 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01F17-206 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01F17-00 |
filingDate | 2017-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106865596-B |
titleOfInvention | The preparation method of spherical cerium oxide dispersion liquid |
abstract | The present invention relates to a kind of preparation methods of spherical cerium oxide dispersion liquid.Manganese ion of the present invention promotes the growth of ceria spherical shape in cryogenic conditions, and the spherical cerium oxide dispersion liquid of preparation, good dispersion, particle size can be widely applied to ultravioletlight screening, chemically mechanical polishing, catalyst in 50-150nm.The preparation process is quick, simply, at low cost, can be mass. |
priorityDate | 2017-03-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |