http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106811117-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-385 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D7-65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-05 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-63 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D7-61 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G77-385 |
filingDate | 2016-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-05-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106811117-B |
titleOfInvention | A kind of long-acting super-hydrophobic anti-pollution flashover coating of improvement slow-release |
abstract | The invention discloses a kind of improvement long-acting super-hydrophobic anti-pollution flashover coatings of 1 type slow-release to be made of following raw material in parts by weight: 35 ~ 45 parts of hydroxypropyl fluorinated polysiloxane of end, 20 ~ 30 parts of hydrogen-based polysiloxanes of end, 107 55 ~ 65 parts of silicon rubber, 20 ~ 30 parts of hydrophobic type gas-phase silica, 3 ~ 5 parts of nano zine oxide, 2 ~ 4 parts of oily amino oleic acid ester, 4 ~ 6 parts of nanometer calcium carbonate, 1 ~ 3 part of ketoxime type crosslinking agent, 5 ~ 10 parts of talcum powder, 1 ~ 2 part of silane coupling agent, 1 ~ 2 part and 165 ~ 175 parts of organic solvent of deca-BDE;The long-acting super-hydrophobic anti-pollution flashover coating mechanical performance of 1 type slow-release of improvement of the invention is strong, long service life, it can reach 15 years, good flame resistance can reach FV-0 grades, and salt spray resistance ageing properties are good, stain resistant is had excellent performance, its validity still can be played in haze polluting weather, reaches expected anti-fouling effect, avoids the generation of pollution flashover accident. |
priorityDate | 2016-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |