http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106751396-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-035 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-014 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L55-02 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L71-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L21-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L55-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 |
filingDate | 2016-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-03-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106751396-B |
titleOfInvention | A kind of high intensity plastic tray for fork truck and preparation method thereof |
abstract | The invention discloses a kind of high-intensitive plastic tray for fork truck, highstrenghtpiston's Pallet for forklift, it is mixed by the first and second components in 3:5 ratio, the first component is based on its mass fraction including following components: ABS:40-50 parts, glass fibre: 3-7 parts, silica: 15-25 parts, nano aluminium oxide: 1-2 parts, 20-30 parts of polystyrene resin, compatilizer: 1-3 parts, promotor: 1-2 parts;The second component is based on its mass fraction including following components: 25-35 parts of rubber resin, polystyrene resin: 20-30 parts, nano-solution: 3-5 parts, 2-5 parts of hexa, toughener: 10-15 parts, antioxidant: 1-3 parts, dispersing agent: 1-2 parts, coupling agent: 2-5 parts, 3-5 parts of interfacial agents;Manufacturing cost of the present invention is low, long service life, intensity are high. |
priorityDate | 2016-12-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 59.