http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106747091-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00017 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-04 |
filingDate | 2016-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106747091-B |
titleOfInvention | A kind of energy saving and environment friendly masonry mortar |
abstract | The invention belongs to energy conservation and environmental protections, more particularly to a kind of energy saving and environment friendly masonry mortar, comprise the following raw materials by weight percent: phosphorus slag powder 20%-25%, modified alum mud 15%-20%, cement 8%-12%, sticking enhancing water-loss reducer 0.01%-0.05%, aluminium-magnesium silicate 0.2%-1%, intensity exciting agent 0.02%-0.08%, remaining as river sand.The ingenious accelerating matter using aluminum contained compound in alum mud and phosphorus slag powder of the invention, which are used in conjunction with, makes masonry mortar of the present invention have suitable setting time.The environmental protection pressure and waste discharge burden that waste discharge enterprise can significantly be mitigated, improve the ecological environment. |
priorityDate | 2016-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |