http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106732708-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F2305-10 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-023 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C02F1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J35-004 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J27-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C02F1-30 |
filingDate | 2016-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-05-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106732708-B |
titleOfInvention | Graphite phase carbon nitride nanometer sheet loads single layer Bismuth tungstate nano-sheet heterojunction material and its preparation method and application |
abstract | The invention discloses a kind of graphite phase carbon nitride nanometer sheet load single layer Bismuth tungstate nano-sheet heterojunction materials and its preparation method and application, and the heterojunction material is with g-C 3 N 4 Nanometer sheet is carrier, g-C 3 N 4 Single layer Bi is modified in nanometer sheet 2 WO 6 Nanometer sheet is level laminated structure.Preparation method includes by g-C 3 N 4 Nanometer sheet, cetyl trimethylammonium bromide are added to Bi (NO 3 ) 3 ·5H 2 In O solution, Na is then added 2 WO 4 ·2H 2 Gained mixed liquor is carried out hydro-thermal reaction, obtains heterojunction material of the invention by O solution.Heterojunction material of the invention has many advantages, such as that photocatalytic activity is high, stablizes, can repeatedly use, and preparation method is with easy to operate, cost of material is low, energy consumption is few.Heterojunction material of the invention can be used for the antibiotic in degrading waste water, have many advantages, such as that good degrading effect, application method are simple, easy to operate. |
priorityDate | 2016-11-11-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.