http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106634902-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2111-00724 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-426 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-5086 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-467 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09K8-5083 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B7-36 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-345 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-467 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B7-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K8-508 |
filingDate | 2016-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-08-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106634902-B |
titleOfInvention | The molten hydraulic cementing materials of high temperature resistant theobromine and be used for oil-well cement slurry system |
abstract | The invention discloses the molten hydraulic cementing materials of high temperature resistant theobromine and it is used for oil-well cement slurry system, the hydraulic cementing materials is made of by weight following each component: 100 parts of lime stone, 10~15 parts of clay, 2~4 parts of bloodstone, 1~3 part of diatomite, 0.1~2 part of ardealite, 1~2 part of gypsum, 30~35 parts of silicon powder, 0~50 part of Iron Ore Powder, 30~45 parts of calcium carbonate.The oil-well cement slurry system prepared by the hydraulic cementing materials includes: 100 parts of cementitious material, 0~1.5 part of kayexalate, 3~6 parts of 2- acrylamide-2-methyl propane sulfonic, 0.5~0.8 part of 2- acrylamide-2-methyl propane sulfonic acrylic copolymer; 1~1.5 part of butadiene-styrene latex; 0.01~0.5 part of dimethicone, 35~50 parts of water.Present invention process is convenient, low in cost, keeps good sedimentation stability in the hot environment of 80 DEG C~130 DEG C of underground by the physical suspension ability of material granule itself, is expected to be applied to the fields such as oil/gas well reservoir temporarily closes, water blockoff, unconventional gas reservoir are cemented the well. |
priorityDate | 2016-12-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 52.