http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106631638-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C06B23-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C06B23-00 |
filingDate | 2017-01-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-07-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106631638-B |
titleOfInvention | A method of improving explosive radiation aging resistant |
abstract | It is to add the polymer of pyrocatechol substance in explosive, the content of the polymer of the pyrocatechol substance of addition accounts for the mass fraction 0.01%~50% of explosive the invention discloses a kind of method improving explosive radiation aging resistant.The present invention improves the simple for process of explosive radiation aging resistant, the polymer of the DOPA substance with catechu phenol functional group of certain content need to be only added in the formula of itself, addition form is unlimited, it can directly add, can also be added polymer by the way of energetic material in situ Polymerization.The present invention can significantly improve the performance of the radiation aging resistant of explosive, the fundamental characteristics such as crystal shape, density and mechanical sensitivity that can in batches prepare on a large scale, and not interfere with material. |