http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106587694-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B2201-50 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B28-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C04B40-0039 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B28-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B22-06 |
filingDate | 2016-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-06-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106587694-B |
titleOfInvention | A kind of solid exciting agent and its preparation process |
abstract | The present invention now provides a kind of solid exciting agent, and each raw material and parts by weight are respectively as follows: 5-50 parts of alkali metal hydroxide;50-95 parts of water glass solution;0.01-3 parts of additive;Alkali metal hydroxide be sodium hydroxide, potassium hydroxide, lithium hydroxide it is one or more;The additive be crystal seed, sodium aluminate it is one or two kinds of;The present invention can form the short chain state that silicon oxygen aluminium (- Si-O-Al-) is connected with the silicate in waterglass using aluminate, be conducive to the formation of geo-polymer, improve the launching efficiency of exciting agent, improve the stability of solid exciting agent. |
priorityDate | 2016-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |