http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106575008-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G02F1-1335 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02B5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G02F1-1335 |
filingDate | 2015-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-12-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106575008-B |
titleOfInvention | Method for producing polarizing film |
abstract | The invention provides a method for manufacturing a polarizing film, which sequentially comprises the following steps: a swelling treatment step of conveying a long polyvinyl alcohol resin film having a thickness of 65 μm or less while winding the polyvinyl alcohol resin film from a raw material roll, thereby immersing the polyvinyl alcohol resin film in a swelling bath and then taking out the polyvinyl alcohol resin film; and a dyeing treatment step of immersing the film drawn out from the swelling bath in a dyeing bath and then drawing out the film, wherein a curl angle of at least one of both ends in a film width direction when the polyvinyl alcohol resin film is immersed in the swelling bath is less than 90 °. |
priorityDate | 2014-08-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |