http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106574446-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H17-11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H19-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D21H23-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B65D65-42 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 |
filingDate | 2015-08-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106574446-B |
titleOfInvention | The manufacturing method of paper composite body, packaging material and paper composite body |
abstract | There is provided oil resistivity, water resistance and the excellent paper composite body of water vapo(u)r transmission, wherein when assigning oil resistivity, oil resistivity can be being improved not increasing the usage amount of the oil-proof composition for the oil-proof composition of 6 Polyfluoroalkyls below using with carbon atom number.The present invention is paper composite body, with 1000g/m 2 Above water vapo(u)r transmission, the paper composite body have for 24 hours:Air permeance resistance is 1000 seconds or less and tightness is 0.5g/cm 3 Above and 1.0g/cm 3 Base paper below;And it is formed in the resistance to oil reservoir at least one surface side of the base paper;Above-mentioned resistance to oil reservoir includes specific ethylene-vinyl alcohol based polymer (A) and the cationic fluorine copolymer (B) with specific 2 kinds of structural units;The content of cationic fluorine copolymer (B) for 100 mass parts of vinyl alcohol system polymer (A) is 5 mass parts or more and 50 is below mass part;The lamination amount of above-mentioned resistance to oil reservoir is calculated as 0.1g/m with dry mass conversion 2 Above and 3.0g/m 2 Below. |