http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106573991-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ecc58e5fd0006c472fea1ec2f879638c |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2220-30 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09J101-286 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M10-052 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-13 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08B11-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-622 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-587 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M4-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L1-286 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D101-286 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D5-24 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08B11-12 |
filingDate | 2015-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_36a4dd3c6db598910af414ad47eb3a14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_266075894ec196ebc053bdb983d3647b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fbb925fb70a26be328e3422f2cd1283d |
publicationDate | 2017-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106573991-A |
titleOfInvention | Method for producing carboxymethyl cellulose salt for electrode of nonaqueous electrolyte secondary battery, electrode for nonaqueous electrolyte secondary battery, and nonaqueous electrolyte secondary battery |
abstract | The object of the present invention is to provide a carboxymethylcellulose salt for an electrode of a non-aqueous electrolyte secondary battery, which can prevent defects such as streaks and pinholes on the coated surface of the electrode and can combine excellent adhesion to a current collector Strength or adhesive strength between active substances. A production method comprising the following steps: (1) an alkali cellulose reaction step, which uses a mixed solvent with a mixing ratio (mass ratio) of alcohol with a carbon number of 3 or less and water of 75:25 to 95:5, and The concentration of alkali relative to water is 25% to 40% by mass; (2) etherification reaction step, which is carried out under the excess of alkali, and the excess of alkali is 0.2 mole per anhydroglucose unit of the cellulose ~0.5 moles; (3) neutralization step, after the etherification reaction is finished, adding acid to adjust the pH value of the reaction mixture to 6.0 ~ 8.0; and (4) heating step, after the neutralization step is finished , removing the mixed solvent, adding a base to adjust the pH of the reaction mixture to 8.0-9.0, and then performing heat treatment at 40°C-70°C for 30 minutes-120 minutes. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-109980295-A |
priorityDate | 2014-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 68.