http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106542585-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2002-72 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2004-03 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01P2006-40 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01G53-006 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G01N27-48 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G01N27-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01G53-00 |
filingDate | 2016-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2018-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2018-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106542585-B |
titleOfInvention | A kind of preparation method of cobalt nickel bimetal sulfide |
abstract | The invention provides a kind of preparation method of cobalt nickel bimetal sulfide, soluble nickel salt and soluble cobalt are dissolved in the ethylene glycol containing cationic surfactant, ultrasonic vibration is completely dissolved to form clear solution, sulphur source compound is then added, continues ultrasound until sulphur source compound is completely dissolved acquisition mixed solution;The mixed solution obtained in step 1 is transferred in autoclave, autoclave sealing is placed in 1~12h of reaction at 60 DEG C~180 DEG C, naturally cool to room temperature, centrifuge and use deionized water and absolute ethyl alcohol alternately wash, black powder is dried to obtain, that is, cobalt nickel bimetal sulfide is made.The present invention is dissolved in the pattern for removing cobalt nickel bimetal sulfide in ethylene glycol solution by cationic surfactant cetyl trimethylammonium bromide, cobalt nickel bimetal sulfide is network hollow microsphere pattern, the pattern electric conductivity is good, the effect of enzyme immobilization is good, can be used in organophosphorus pesticide biology sensor. |
priorityDate | 2016-10-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |