http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106513011-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J2523-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D2258-0283 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01J23-8892 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B01D53-8628 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-90 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J23-889 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D53-56 |
filingDate | 2016-11-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2021-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2021-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106513011-B |
titleOfInvention | Metal composite oxide SCR flue gas denitration catalyst and preparation method thereof |
abstract | The invention discloses a metal composite oxide SCR flue gas denitration catalyst and a preparation method thereof. The catalyst is prepared by taking environment-friendly transition metals Fe, Mn and Zr as raw materials and adopting a simple coprecipitation method, wherein a coprecipitator is ammonia water, the coprecipitation method is sequential addition, the ammonia water dropping speed is high, the roasting temperature is 300-700 ℃, and the roasting atmosphere is air. The metal composite oxide SCR flue gas denitration catalyst realizes high airspeed (35000 h) within the range of 130-400 DEG C ~1 ) More than 80% NH, up to 100% NH under the condition 3 -SCR denitration activity. |