http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106480317-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0b75a05785dbfd86d27a87ddcdc5a524 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d8f58294a0b06cb7039c720bd7677d6e |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0069 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B7-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C22B15-0091 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B15-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C22B7-00 |
filingDate | 2016-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7fdd512dc49f77d1b1ea3e94349ea73e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5e19b847495d5999bcd0ada9d52838ec http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72557533011af38b294e838301d9b166 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d917ce8f10e853f827e3c62d9402aecf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bcbcb6bf90298dd6c90e8c05bd078c11 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e96286ef16123535223aa8e00e52be74 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd3890af5e1f485964b02f7c63c739e4 |
publicationDate | 2017-03-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106480317-A |
titleOfInvention | A kind of technique simultaneously processing the high iron alloy material in copper smelting-furnace bottom and useless technical hydrochloric acid comprehensive recovery of iron, copper and other noble metal |
abstract | The invention discloses one kind processes the high iron alloy material in copper smelting-furnace bottom and useless technical hydrochloric acid simultaneously, and comprehensive recovery of iron, copper and the technique of other noble metal, this technique is with the useless technical hydrochloric acid of organic chemical industry's Industrial Output as leaching agent, the smelting furnace bottom alloy material of high Fe content is directly leached, obtain iron content leachate and Concentration of Gold, the leached mud of silver, iron content leachate is carried out with impulse ultrasound coupling iron plane again and spends reduction purification, valuable element dissolving being entered in leachate is strengthened in displacement entrance replacement slag by ultrasonic coupling, arsenic is especially made to enter in replacement slag with the stable state of copper arsenic alloy phase, avoid AsH 3 The generation of gas.And obtained the FeCl meeting Standard 3 Water purification agent product.This technique whole process no waste water, waste residue produce, achieve the high iron alloy material in copper smelting-furnace bottom and the full dose of useless technical hydrochloric acid utilizes, technological process closed cycle, has that adaptability to raw material is strong, technological process simple, the valuable element response rate is high, the outstanding advantages of clean environment firendly. |