http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-106467670-B
Outgoing Links
Predicate | Object |
---|---|
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-001 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2201-011 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-0806 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K7-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22F9-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 |
filingDate | 2016-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2019-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2019-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | CN-106467670-B |
titleOfInvention | A kind of preparation method of silver nanoparticle mixed fillers modified silicon rubber conducing composite material |
abstract | The present invention relates to nanocomposite technical fields, to solve the nano-Ag particles of conventional method preparation there is high surface energy easily to reunite, compatibility between silver nano-grain and silicone rubber matrix is poor, make its be not easy it is evenly dispersed in the base and the problem of influence the comprehensive performance of composite material, the invention proposes a kind of preparation methods of silver nanoparticle mixed fillers modified silicon rubber conducing composite material, nano-Ag particles are prepared using chemical reduction method, it is modified that surface is carried out with silane coupling agent, it is allowed to be relatively uniformly dispersed throughout in organic solvent, and combine silver nanowires, silver nano-grain and its mixed fillers are distributed in silicone rubber matrix using solution blending process, prepare the elastic silicone rubber nanocomposite of superior electrical conductivity energy.The composite material not only has the advantages that stable resistor time characteristic, higher temperature limit and temperature-coefficient of electrical resistance are controllable, but also has both the high resiliency of rubber material. |
priorityDate | 2016-09-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |